Simultaneous improvements of strength and toughness in topologically interlocked ceramics
Mohammad Mirkhalaf1, Tao Zhou1, Francois Barthelat2
1Department of Mechanical Engineering, McGill University, Montreal, QC H3A 2K6, Canada.
Abstract:
Topologically interlocked materials (TIMs) are an emerging class of architectured materials based on stiff building blocks of well-controlled geometries which can slide, rotate, or interlock collectively providing a wealth of tunable mechanisms, precise structural properties, and functionalities. TIMs are typically 10 times more impact resistant than their monolithic form, but this improvement usually comes at the expense of strength. Here we used 3D printing and replica casting to explore 15 designs of architectured ceramic panels based on platonic shapes and their truncated versions. We tested the panels in quasi-static and impact conditions with stereoimaging, image correlation, and 3D reconstruction to monitor the displacements and rotations of individual blocks. We report a design based on octahedral blocks which is not only tougher (50×) but also stronger (1.2×) than monolithic plates of the same material. This result suggests that there is no upper bound for strength and toughness in TIMs, unveiling their tremendous potential as structural and multifunctional materials. Based on our experiments, we propose a nondimensional "interlocking parameter" which could guide the exploration of future architectured systems.
More Related Videos
06:53Additive Manufacturing of Functionally Graded Ceramic Materials by Stereolithography
Published on: January 25, 2019
08:29Multi-material Ceramic-Based Components – Additive Manufacturing of Black-and-white Zirconia Components by Thermoplastic 3D-Printing (CerAM - T3DP)
Published on: January 7, 2019
Related Concept Videos
Toughness and Hardness of Aggregate
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
The Equilibrium Binding Constant and Binding Strength
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...