Phase-field modeling for pH-dependent general and pitting corrosion of iron

Chisa Tsuyuki1, Akinori Yamanaka2, Yasushi Ogimoto3

  • 1Department of Mechanical Systems Engineering, Graduate School of Engineering, Tokyo University of Agriculture and Technology, 2-24-16, Naka-cho, Koganei-shi, Tokyo, 184-8588, Japan.

Scientific Reports
|August 26, 2018
PubMed

Related Concept Videos

Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
28.4K
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
583
Phase Diagrams02:39

Phase Diagrams

A phase diagram combines plots of pressure versus temperature for the liquid-gas, solid-liquid, and solid-gas phase-transition equilibria of a substance. These diagrams indicate the physical states that exist under specific conditions of pressure and temperature and also provide the pressure dependence of the phase-transition temperatures (melting points, sublimation points, boiling points). Regions or areas labeled solid, liquid, and gas represent single phases, while lines or curves represent...
50.3K
Phase Transitions02:31

Phase Transitions

Whether solid, liquid, or gas, a substance's state depends on the order and arrangement of its particles (atoms, molecules, or ions). Particles in the solid pack closely together, generally in a pattern. The particles vibrate about their fixed positions but do not move or squeeze past their neighbors. In liquids, although the particles are closely spaced, they are randomly arranged. The position of the particles are not fixed—that is, they are free to move past their neighbors to...
23.2K
Frequency-dependent Selection01:21

Frequency-dependent Selection

When the fitness of a trait is influenced by how common it is (i.e., its frequency) relative to different traits within a population, this is referred to as frequency-dependent selection. Frequency-dependent selection may occur between species or within a single species. This type of selection can either be positive—with more common phenotypes having higher fitness—or negative, with rarer phenotypes conferring increased fitness.
24.1K
Temperature Dependence on Reaction Rate02:55

Temperature Dependence on Reaction Rate

The Collision Theory
Atoms, molecules, or ions must collide before they can react with each other. Atoms must be close together to form chemical bonds. This premise is the basis for a theory that explains many observations regarding chemical kinetics, including factors affecting reaction rates.
The collision theory is based on the postulates that (i) the reaction rate is proportional to the rate of reactant collisions, (ii) the reacting species collide in an orientation allowing contact between...
89.1K