Photocatalysis and Hydrogen Evolution of Al- and Zn-Doped TiO2 Nanotubes Fabricated by Atomic Layer Deposition
Chung-Yi Su1, Li-Chen Wang1, Wei-Szu Liu1
1Department of Materials Science and Engineering , National Tsing Hua University , 101 Section 2, Kuang-Fu Rd. , Hsinchu 30013 , Taiwan.
Abstract:
Highly homogeneous Al- and Zn-doped TiO2 nanotubes were fabricated by atomic layer deposition (ALD) via nanolaminated stacks of binary layers of TiO2/Al2O3 and TiO2/ZnO, respectively. The bilayers were alternately deposited on the polycarbonate (PC) membrane template by ALD with various cyclic sequences. The nanotubes in a length of 20 μm and a diameter of 220 nm were obtained after removal of the PC membrane by annealing at 450 °C. The effects of doping composition on the photocatalytic and photoelectrochemical (PEC) activities were investigated. Increasing the Al doping reduced the photocatalytic activity of TiO2 due to formation of charge recombination sites and reduction of hydroxide radicals. In contrast, there was an optimal range of Zn doping to get enhanced photocatalytic activity and higher PEC efficiency. With a doping ratio of 0.01, the hydrogen production rate from water splitting was 6 times higher than that of commercial P25 TiO2. The energy-band diagram of Zn-doped TiO2 determined by ultraviolet photoelectron spectroscopy revealed shift up of the Fermi level to provide more electrons to the conduction band. The photoinduced trapped electrons and holes were detected in Zn-doped TiO2 by in situ electron paramagnetic resonance spectroscopy, which revealed that Ti3+ sites on the surface and surface oxygen vacancies played a key role in promoting the photocatalytic process.
Related Concept Videos
Hydrogen Bonds
Hydrogen Bonds Control the World!
Because hydrogen has very weak electronegativity when it binds with a strongly electronegative atom, such as oxygen or nitrogen, electrons in the bond are unequally shared....
The Evidence for Evolution
Atomic Orbitals
Convergent Evolution
The Atomic Theory of Matter
Hybridization of Atomic Orbitals I