Mechanical properties of cancellous tissue in compression test and nanoindentation
Related Experiment Video
Updated: Feb 4, 2026

Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
Grzegorz Kokot1, Anna Makuch2, Konstanty Skalski2
1Silesian University of Technology, Gliwice, Poland.
Abstract:
The goal of the study was to determine material constants of cancellous tissue in a compression test taking into account stress-strain characteristics. The nineteen test samples were resected from a femoral head of a patient qualified for a hip replacement surgery. During the compression tests, load-displacement curves were evaluated and stress-strain characteristics (𝜎-𝜀) of the cancellous bone tissue were calculated. A special one-touch extensometer was used. The use of an extensometer improves the displacement measurement accuracy with respect to the measurement using standard crosshead. The obtained values of the mechanical parameters as well as the stress-strain curves are the basis for further research going into the development of bone tissue constitutive equations.
Related Concept Videos
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...
Physical and Chemical Properties of Matter
Properties of Transition Metals
The Quantum-Mechanical Model of an Atom
Reaction Mechanisms
For instance, the decomposition of ozone appears to follow a mechanism with two steps:
General Properties of Solutions