Related Experiment Video
Updated: Feb 3, 2026

Ensemble Force Spectroscopy by Shear Forces
Published on: July 26, 2022
Shear bond strength of luting cements to fixed superstructure metal surfaces under various seating forces
Fusun Ozer1, Elif Pak-Tunc2, Nesrin Esen Dagli1
1School of Dental Medicine, University of Pennsylvania, Philadelphia, PA, USA.
Purpose:
In this study, the shear bond strengths (SBS) of luting cements to fixed superstructure metal surfaces under various seating forces were investigated.
Materials And Methods:
Seven different cements [Polycarboxylate (PCC), Glass-Ionomer (GIC), Zinc phospahate (ZPC), Self-adhesive resin (RXU), Resin (C&B), and Temporary cements ((RXT) and (TCS))] were bonded to a total number of 224 square blocks (5×5×3 mm) made of one pure metal [Titanium (CP Ti) and two metal alloys [Gold-Platinum (Au-Pt) and Cobalt-Chrome (Co-Cr)] under 10 N and 50 N seating forces. SBS values were determined and data were analyzed with 3-way ANOVA. Pairwise comparisons and interactions among groups were analyzed with Tukey's simultaneous confidence intervals.
Results:
Overall mean scores indicated that Co-Cr showed the highest SBS values (1.96±0.4) (P<.00), while Au-Pt showed the lowest among all metals tested (1.57±0.4) (P<.00). Except for PCC/CP Ti, RXU/CP Ti, and GIC/Au-Pt factor level combinations (P<.00), the cements tested under 10 N seating force showed no significantly higher SBS values when compared to the values of those tested under 50 N seating force (P>.05). The PCC cement showed the highest mean SBS score (3.59±0.07) among all cements tested (P<.00), while the resin-based temporary luting cement RXT showed the lowest (0.39±0.07) (P<.00).
Conclusion:
Polycarboxylate cement provides reliable bonding performance to metal surfaces. Resin-based temporary luting cements can be used when retrievability is needed. GIC is not suitable for permanent cementation of fixed dental prostheses consisting of CP Ti or Au-Pt substructures.
Related Concept Videos
Bonding in Metals
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Metal-Ligand Bonds
In these complexes, transition metals form coordinate covalent bonds, a kind of Lewis acid-base interaction in which both of the electrons in the bond are contributed by a donor (Lewis base) to an electron acceptor (Lewis acid). The Lewis acid in...
Bonding and Strength of Aggregate
Normal and Shear Force
Metallic Solids
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability....