Higher Strength and Ductility than Diamond: Nanotwinned Diamond/Cubic Boron Nitride Multilayer
Abstract:
Recently, the nanotwinned structure has attracted considerable attention because of unprecedented improvement in its mechanical properties, thermal stability, and other properties. Here, we introduce the nanotwinned structure between two superhard materials [diamond and cubic boron nitride (cBN)] and obtain a nanotwinned diamond/cBN multilayered material with ultrahigh strength and unprecedented ductility. Under continuous shear deformation, the stress and total energy in the material develop in a zigzag way because of atomic reconfiguration. Further research shows that atomic reconfiguration occurs preferentially in the cBN region, followed by that in the diamond region by partial slip, and finally occurs at the interface through alternate "exchange" of the positions of C and B atoms. This multilevel stress release model can account for the significant increase in the strain range and peak stress of nanotwinned materials. These results could provide available information for the design of superhard materials with multilevel resistance to plastic deformation.
Related Concept Videos
Stress-Strain Diagram - Ductile Materials
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
The Equilibrium Binding Constant and Binding Strength