Abstract:
The nanomechanical properties and nanoindentation responses of bismuth selenide (Bi₂Se₃) thin films are investigated in this study. The Bi₂Se₃ thin films are deposited on c-plane sapphire substrates using pulsed laser deposition. The microstructural properties of Bi₂Se₃ thin films are analyzed by means of X-ray diffraction (XRD). The XRD results indicated that Bi₂Se₃ thin films are exhibited the hexagonal crystal structure with a c-axis preferred growth orientation. Nanoindentation results showed the multiple "pop-ins" displayed in the loading segments of the load-displacement curves, suggesting that the deformation mechanisms in the hexagonal-structured Bi₂Se₃ films might have been governed by the nucleation and propagation of dislocations. Further, an energetic estimation of nanoindentation-induced dislocation associated with the observed pop-in effects was made using the classical dislocation theory.
More Related Videos
08:58Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
07:08Film Control to Study Contributions of Waves to Droplet Impact Dynamics on Thin Flowing Liquid Films
Published on: August 18, 2018