Detection of Friction Stir Welding Defects of AA1060 Aluminum Alloy Using Specific Damping Capacity

Waheed Sami AbuShanab1, Essam B Moustafa2

  • 1Marine Engineering Department, Faculty of Maritime Studies and Marine Engineering, King Abdulaziz University, Jeddah 21589, Saudi Arabia. wabushanab@kau.edu.sa.

Related Concept Videos

Lung Capacity01:47

Lung Capacity

The air in the lungs is measured in volumes and capacities. Lung volume measures reflect the amount of air taken in, released, or left over after a lung function, like a single inhalation. Lung capacity measures are sums of two or more lung volume measures.
56.3K
Damped Oscillations01:07

Damped Oscillations

In the real world, oscillations seldom follow true simple harmonic motion. A system that continues its motion indefinitely without losing its amplitude is termed undamped. However, friction of some sort usually dampens the motion, so it fades away or needs more force to continue. For example, a guitar string stops oscillating a few seconds after being plucked. Similarly, one must continually push a swing to keep a child swinging on a playground.
Although friction and other non-conservative...
7.2K
Types of Damping01:20

Types of Damping

If the amount of damping in a system is gradually increased, the period and frequency start to become affected because damping opposes, and hence slows, the back and forth motion (the net force is smaller in both directions). If there is a very large amount of damping, the system does not even oscillate; instead, it slowly moves toward equilibrium. In brief, an overdamped system moves slowly towards equilibrium, whereas an underdamped system moves quickly to equilibrium but will oscillate about...
7.7K
Magnetic Damping01:17

Magnetic Damping

Eddy currents can produce significant drag on motion, called magnetic damping. For instance, when a metallic pendulum bob swings between the poles of a strong magnet, significant drag acts on the bob as it enters and leaves the field, quickly damping the motion.
If, however, the bob is a slotted metal plate, the magnet produces a much smaller effect. When a slotted metal plate enters the field, an emf is induced by the change in flux; however, it is less effective because the slots limit the...
1.1K
Kinetic Friction01:26

Kinetic Friction

Consider a truck trying to pull a stationary car. As the truck exerts a force on the car, static friction is created at the point of contact between the two surfaces. This frictional force resists the car's movement and keeps it at rest. However, when the applied force by the truck surpasses the limiting static frictional force, an interesting phenomenon occurs. The frictional force at the interface reduces to a lower value, known as the kinetic frictional force. At this point, the car...
1.4K
Types of Friction Problems01:27

Types of Friction Problems

Friction is an essential concept in physics, engineering, and everyday life. It is the force that opposes the relative motion or tendency of such motion between two surfaces in contact. One of the most common types of friction encountered in various applications is dry friction. Dry friction problems can be broadly categorized into three types, each with unique characteristics and challenges.
The first type of dry friction problem involves situations where there is no apparent impending motion....
987