Experimental and Data Analysis Workflow for Soft Matter Nanoindentation
Published on: January 18, 2022
Nanoindentation of Soft Biological Materials
1School of Mechanical and Aerospace Engineering, Jilin University, Changchun 130025, China. qianlong17@mails.jlu.edu.cn.
Abstract:
Nanoindentation techniques, with high spatial resolution and force sensitivity, have recently been moved into the center of the spotlight for measuring the mechanical properties of biomaterials, especially bridging the scales from the molecular via the cellular and tissue all the way to the organ level, whereas characterizing soft biomaterials, especially down to biomolecules, is fraught with more pitfalls compared with the hard biomaterials. In this review we detail the constitutive behavior of soft biomaterials under nanoindentation (including AFM) and present the characteristics of experimental aspects in detail, such as the adaption of instrumentation and indentation response of soft biomaterials. We further show some applications, and discuss the challenges and perspectives related to nanoindentation of soft biomaterials, a technique that can pinpoint the mechanical properties of soft biomaterials for the scale-span is far-reaching for understanding biomechanics and mechanobiology.
Related Concept Videos
What is Conservation Biology?
Biological Effects of Radiation
Members Made of Elastoplastic Material
As the bending moment...
Genetic Material
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Synthetic Biology
Golden rice
Golden rice is a genetically modified...