Effect of Zn/Mg Ratios on Microstructure and Stress Corrosion Cracking of 7005 Alloy
Shuai Wang1, Binghui Luo2, Zhenhai Bai3
1Key Laboratory for Nonferrous Materials (MOE), School of Materials Science and Engineering, Central South University, Changsha 410083, China. 163101020@csu.edu.cn.
Abstract:
The effects of different Zn/Mg ratios on the microstructure, mechanical properties and resistance of stress corrosion cracking of peak-aged 7005 aluminum alloy were investigated. It was found that the Zn/Mg ratio played a very important role in controlling the aging time, the electrical conductivity of the hardness peak point and the resistance of stress corrosion cracking of the alloy. With the increase of Zn/Mg ratio (wt. %), the time taken by the alloy to achieve the peak hardness value gradually increases aging at 120 °C. When the Zn/Mg ratio is in the range from 2.27% to 2.62%, the precipitate phase of the alloy after peak-aged is mainly dominated by smaller disc-like η' phase and GP I (Guinier Preston) zones, the grain boundary precipitates are slender and continuous and the PFZ (precipitate free zones) is narrow. However when this value is in the range from 3.01% to 4.08%, precipitation phase in matrix of the alloy is mainly composed of short-rod η' phase and GP II zones, the precipitation phases within the grain boundary are large and distribute intermittently and the PFZ is narrower. The results of SSRT (slow strain rate tests) show that when Zn/Mg ≥ 3.61, the 7005 aluminum alloy at peak-aged has good resistance of stress corrosion cracking in 3.5% NaCl + 0.5% H₂O₂ aqueous solution. However, when Zn/Mg ≤ 3.01, the strength of the alloy sharply decreases in 3.5% (wt. %) NaCl + 0.5% (wt. %) H₂O₂ aqueous solution.
More Related Videos
07:37Full-field Strain Measurements for Microstructurally Small Fatigue Crack Propagation Using Digital Image Correlation Method
Published on: January 16, 2019
14:51An Available Technique for Preparation of New Cast MnCuNiFeZnAl Alloy with Superior Damping Capacity and High Service Temperature
Published on: September 23, 2018
Related Concept Videos
Corrosion
Corrosion of Reinforcement
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Types of Non-structural Cracks in Concrete
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Poisson's Ratio
Odds Ratio
Hazard Ratio
For example, in a clinical trial...