Degradation behaviors and cytocompatibility of Mg/β-tricalcium phosphate composites produced by spark plasma
Kai Narita1,2, Qiaomu Tian2,3, Ian Johnson2
1Department of Metallurgy & Ceramics Science, Graduate School of Science & Engineering, Tokyo Institute of Technology, Tokyo, Japan.
Abstract:
Magnesium (Mg)-based materials have shown great potentials for bioresorbable implant applications. Previous studies showed that Mg with 10 and 20 vol % β-tricalcium phosphate (β-TCP) composites produced by spark plasma sintering, improved mechanical properties when compared with pure Mg. The objectives of this study were to evaluate the degradation behaviors of Mg/10% β-TCP and Mg/20% β-TCP composites in revised stimulated body fluid (rSBF), and to determine their cytocompatibility with bone marrow derived mesenchymal stem cells (BMSCs) using the direct culture method. During the 11 days of immersion in rSBF, Mg/β-TCP composites showed different degradation behaviors at different immersion periods, that is, the initial stage (0-1 hr), the mid-term stage (1 hr to 2 days), and the long-term stage (2-11 days). The counter effects of mass loss due to microgalvanic corrosion and mass gain due to deposition of Ca-P containing layers resulted in slower Mg2+ ion release for Mg/20% β-TCP than Mg/10% β-TCP in the mid-term, but eventually 16% mass loss for Mg/20% β-TCP and 10% mass loss for Mg/10% β-TCP after 11 days of immersion. The in vitro studies with BMSCs showed the highest cell adhesion density (i.e., 68% of seeding density) on the plate surrounding the Mg/10% β-TCP sample, that is, under the indirect contact condition of direct culture. The β-TCP showed a positive effect on direct adhesion of BMSCs on the surface of Mg/β-TCP composites. This study elucidated the degradation behaviors and the cytocompatibility of Mg/β-TCP composites in vitro; and, further studies on Mg/ceramic composites are needed to determine their potential for clinical applications. © 2019 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 107B: 2238-2253, 2019.
More Related Videos
07:04Confocal Time Lapse Imaging as an Efficient Method for the Cytocompatibility Evaluation of Dental Composites
Published on: November 9, 2014
10:41The Effect of Charging and Discharging Lithium Iron Phosphate-graphite Cells at Different Temperatures on Degradation
Published on: July 18, 2018
Related Concept Videos
Composition of Blood Plasma
Regulated Protein Degradation
Protein degradation plays two important roles in the cells. It helps to protect cells from misfolded or damaged proteins before they lead to a...
Regulated Protein Degradation
Proteins: From Genes to Degradation
Transcription is the synthesis of RNA...
Proteins: From Genes to Degradation
Phosphate Buffer
Sodium dihydrogen phosphate does not fully dissociate in neutral or acidic solutions. When a strong base, such as sodium hydroxide (NaOH), is introduced into the solution, sodium dihydrogen phosphate...