Optical properties and flexural strength of translucent zirconia layered with high-translucent zirconia
Takanori Sakai1,2, Toru Sato1, Ryuichi Hisanaga1
1Department of Fixed Prosthodontics, Tokyo Dental College.
Abstract:
This study investigated the optical properties and flexural strength of translucent TZP layered with high-translucent PSZ using resin cement of various shades. Zirconia specimens (translucent TZP; Zpex and high-translucent PSZ; ZpexSmile) were 13 mm in diameter, layered at thickness ratios of 0.3/0.7, 0.5/0.5, and 0.7/0.3 mm (ZpexSmile/Zpex), and then luted using resin cement of 3 shades. Monolithic specimens of both were used as controls. CIE L*a*b* color coordinates and translucency parameter (TP) were evaluated as optical properties. Biaxial flexural strength was also determined as a mechanical evaluation. The a* and b* values of layered specimens varied depending on the shade of cement. TP values were not affected by shade of cement and thickness ratio. The biaxial flexural strength was intermediate value between both monolithic specimens. The layering method of zirconia with various translucencies using resin cement of different shades can improve color expression while maintaining clinically sufficient flexural strength.
More Related Videos
07:13High Temperature Fabrication of Nanostructured Yttria-Stabilized-Zirconia YSZ Scaffolds by In Situ Carbon Templating Xerogels
Published on: April 16, 2017
11:25A Millimeter Scale Flexural Testing System for Measuring the Mechanical Properties of Marine Sponge Spicules
Published on: October 11, 2017
Related Concept Videos
Properties of Enantiomers and Optical Activity
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
The Equilibrium Binding Constant and Binding Strength