Cycling-Induced Capacity Increase of Graphene Aerogel/ZnO Nanomembrane Composite Anode Fabricated by Atomic Layer
Dingrun Wang1, Yalan Li1, Yuting Zhao1
1Department of Materials Science, Fudan University, Shanghai, 200433, People's Republic of China.
Abstract:
Zinc oxide (ZnO) nanomembranes/graphene aerogel (GAZ) composites were successfully fabricated via atomic layer deposition (ALD). The composition of GAZ composites can be controlled by changing the number of ALD cycles. Experimental results demonstrated that the anode made from GAZ composite with ZnO nanomembrane of 100 ALD cycles exhibited highest specific capacity and best rate performance. A capacity increase of more than 2 times during the first 500 cycles was observed, and a highest capacity of 1200 mAh g-1 at current density of 1000 mA g-1 was observed after 500 cycles. On the basis of detailed electrochemical investigations, we ascribe the remarkable cycling-induced capacity increase to the alloying process accompanied by the formation of a polymer layer resulting from kinetically activated electrolyte degradation at low voltage regions.
More Related Videos
10:39Preparation of ZnO Nanorod/Graphene/ZnO Nanorod Epitaxial Double Heterostructure for Piezoelectrical Nanogenerator by Using Preheating Hydrothermal
Published on: January 15, 2016
11:10Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
Published on: May 23, 2018
Related Concept Videos
Lung Capacity
Classifying Matter by Composition
According to its composition, the matter can be classified into two broad categories — pure substances and mixtures.
A pure substance is a form of matter that has a constant composition throughout with uniform properties. For example, any sample of sucrose has the same composition and same physical properties, such as melting point, color, and sweetness, regardless of the source from which it is isolated.
A mixture is composed of two or...
The Nitrogen Cycle
The Phosphorus Cycle
What are Biogeochemical Cycles?
The Carbon Cycle