Can Prophylactic Cables Stop Crack Propagation in Revision Arthroplasty: A Biomechanical Study
Lukas S Kuster1, Daniel Marshall2, Christian Fässler3
1Department of Orthopaedic Surgery, Sir Charles Gairdner Hospital, Nedlands, Western Australia, Australia.
Background:
Intraoperative femur fractures are a common complication of revision hip arthroplasty. This study examined the use of a prophylactic cable in stopping a crack from propagating beyond the cable.
Methods:
Seventy sheep femora were prepared. A 5-mm vertical incision was performed. Using a force-controlled materials testing machine, a Wagner shaft was advanced until a crack occurred. Cracks were visualized with green ink. In the first part, the control group without any cable (n = 10) was compared with polyethylene (n = 15) and single CoCr cable (n = 15) groups. The cables were positioned 15 mm distal to the osteotomy. In the second part, three different CoCr configurations were compared, single-wrapped (n = 15), double-wrapped (n = 125), and two separate cables at 10 and 15 mm distal to the osteotomy (n = 15).
Results:
The polyethylene cable stopped only 3 of 15 cracks (20%), whereas the CoCr cable stopped 11 of 15 cracks (73%) (P = .009). The force needed to initiate the crack between the different groups was not significant. Twelve (80%) of 15 cracks were stopped at the level of the cable with two separate CoCr cables and 15 (100%) of 15 cracks with a double-wrapped cable (P = .11).
Conclusion:
This study demonstrated that an elastic cable is not suitable for preventive cabling. The force required to form a crack is not improved with the use of a prophylactic cable placed 10-15 mm below the osteotomy. While the results on the different configurations were not conclusive, the double-wrapped cable was able to stop all cracks from progressing distally.
More Related Videos
Related Concept Videos
Cable: Problem Solving
Cable Subjected to Its Own Weight
A generalized loading function is employed to analyze a cable subjected to its own weight. This function considers the force acting along the cable's arc length rather than its projected length, providing a more accurate...
Types of Non-structural Cracks in Concrete
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
Energy Stored In A Coaxial Cable
In the simplest form, a coaxial cable can be represented by two long hollow concentric cylinders in which the current flows in opposite directions. The magnetic field inside and outside the coaxial cable is determined by using Ampère's law. The magnetic field inside...
Cable Subjected to Concentrated Loads
Cable Subjected to a Distributed Load