Design of InZnSnO Semiconductor Alloys Synthesized by Supercycle Atomic Layer Deposition and Their Rollable

Jiazhen Sheng1, TaeHyun Hong1, DongHee Kang2

  • 1Division of Materials Science and Engineering , Hanyang University , 222, Wangsimni-ro , Seongdong-gu, Seoul 04763 , Republic of Korea.

Related Concept Videos

Semiconductors01:22

Semiconductors

There is variation in the electrical conductivity of materials - metals, semiconductors, and insulators that are showcased with the help of the energy band diagrams.
Metals such as copper (Cu), zinc (Zn), or lead (Pb) have low resistivity and feature conduction bands that are either not fully occupied or overlap with the valence band, making a bandgap non-existent. This allows electrons in the highest energy levels of the valence band to easily transition to the conduction band upon gaining...
1.5K
Design Example: Application of Archimedes' Principle01:11

Design Example: Application of Archimedes' Principle

Archimedes' principle is fundamental in analyzing the buoyant force and stability of floating bodies. In this example, a wooden block with a rectangular section floats in seawater. Based on the block's dimensions, its specific gravity and the specific weight of seawater are used to find the volume of water displaced and the center of buoyancy.
The volume of seawater displaced by the block is determined by first calculating the block's weight. This is done by multiplying the...
828
Atomic Structure01:33

Atomic Structure

Overview
208.6K
Atomic Mass01:52

Atomic Mass

Atoms — and the protons, neutrons, and electrons that compose them — are extremely small. For example, a carbon atom weighs less than 2 × 10−23 g. When describing the properties of tiny objects such as atoms, we use appropriately small units of measure, such as the atomic mass unit (amu). The amu was originally defined based on hydrogen, the lightest element, then later in terms of oxygen. Since 1961, it has been defined with regard to the most abundant isotope of carbon, atoms of which...
70.0K
Atomic Orbitals02:44

Atomic Orbitals

An atomic orbital represents the three-dimensional regions in an atom where an electron has the highest probability to reside. The radial distribution function indicates the total probability of finding an electron within the thin shell at a distance r from the nucleus. The atomic orbitals have distinct shapes which are determined by l, the angular momentum quantum number. The orbitals are often drawn with a boundary surface, enclosing densest regions of the cloud.
43.7K
Types of Semiconductors01:20

Types of Semiconductors

Intrinsic semiconductors are highly pure materials with no impurities. At absolute zero, these semiconductors behave as perfect insulators because all the valence electrons are bound, and the conduction band is empty, disallowing electrical conduction. The Fermi level is a concept used to describe the probability of occupancy of energy levels by electrons at thermal equilibrium. In intrinsic semiconductors, the Fermi level is positioned at the midpoint of the energy gap at absolute zero. When...
1.4K