Preparation and Characterization of Softwood Kraft Lignin Copolymers as a Paper Strength Additive
Zhongming Liu1, Dingding Xu2, Lei Xu3
1State Key Laboratory of Biobased Material and Green Papermaking, Key Laboratory of Pulp & Paper Science and Technology of Shandong Province/Ministry of Education, Qilu University of Technology (Shandong Academy of Sciences), Jinan 250353, China. liuzhongming126@126.com.
Abstract:
Softwood kraft lignin is a renewable type of woody material that can be converted to value-added products, for example, as a paper strength additive in the paper industry. In this study, the monomers of methacryloxyethyltrimethyl ammonium chloride (DMC), acrylic acid (AA), and acrylamide (AM) were grafted on softwood kraft lignin (SKL) to prepare three different SKL copolymers. Fourier-transform infrared, proton nuclear magnetic resonance, charge density, elemental, and molecular weight analyses confirmed that the monomers were successfully grafted onto SKL. The grafting rates of SKL-DMC, SKL-AA, and SKL-AM copolymers were 80.35%, 82.70%, and 79.48%, respectively. The application of SKL copolymers as a paper additive for enhancing paper physical properties was studied. The results indicated that at a 2 wt % dosage of SKL copolymers, the increase in the physical properties of paper is maximum.
More Related Videos
Related Concept Videos
Softwoods and Hardwoods
Preparation of Alcohols via Addition Reactions
The acid-catalyzed addition of water to the double bond of alkenes is a large-scale industrial method used to synthesize low-molecular-weight alcohols. An acidic atmosphere is required to allow the hydrogen in the water molecule to act as an electrophile and attack the double bond in an alkene. The addition of a proton to the double bond creates a carbocation intermediate. The proton preferentially bonds to the less substituted end of the double bond to create a more stable carbocation...
Conjugate Addition (1,4-Addition) vs Direct Addition (1,2-Addition)
Conjugate addition results in a thermodynamically stable product. The reaction retains the stronger C=O bond at the expense of the weaker C=C π bond. The process is slow as the β carbon is less electrophilic than the carbonyl carbon.
Direct addition products are...
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Characteristics and Nomenclature of Copolymers
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...