Dataset on hydrophobicity indices and differential scanning calorimetry thermograms for poly(HEMA)-based hydrogels

Ankita Bhat1,2, Blake Smith1,2, Cerasela-Zoica Dinu3

  • 1Center for Bioelectronics, Biosensors and Biochips (C3B), Department of Biomedical Engineering, Texas A&M University, College Station, TX 77843, USA.

Data in Brief
|June 14, 2019
PubMed

Related Concept Videos

Indicators02:39

Indicators

Certain organic substances change color in dilute solution when the hydronium ion concentration reaches a particular value. For example, phenolphthalein is a colorless substance in any aqueous solution with a hydronium ion concentration greater than 5.0 × 10−9 M (pH < 8.3). In more basic solutions where the hydronium ion concentration is less than 5.0 × 10−9 M (pH > 8.3), it is red or pink. Substances such as phenolphthalein, which can be used to determine the pH of a solution, are...
59.8K
Constant Pressure Calorimetry03:02

Constant Pressure Calorimetry

Calorimetry is a technique used to measure the amount of heat involved in a chemical or physical process or to measure the heat transferred to or from a substance. The heat is exchanged with a calibrated and insulated device called the calorimeter. Calorimetry experiments are based on the assumption that there is no heat exchange between the insulated calorimeter and the external environment. The well-insulated calorimeters prevent the transfer of heat between the calorimeter and its external...
97.4K
Calorimetry01:19

Calorimetry

When objects at different temperatures are placed in contact with each other but isolated from everything else, they attain thermal equilibrium. A container that prevents heat transfer in or out is called a calorimeter, and the use of a calorimeter to make measurements is called calorimetry. Generally, these measurements involve heat or specific heat capacity. The term "calorimetry problem" is used for any problem where the specified objects are thermally isolated from their...
4.3K
Cardiovascular Drugs: Classification based on Therapeutic Indications01:18

Cardiovascular Drugs: Classification based on Therapeutic Indications

Cardiovascular diseases, encompassing a range of conditions, can significantly affect the heart's operations and the overall circulatory system. These conditions impair the heart's ability to pump blood, leading to a deficit in oxygen supply to crucial organs. Anomalies in the heart's electrical system, known as arrhythmias, can cause heartbeats to accelerate or slow down. Usually, heart rates increase during physical activity and decrease while resting or sleeping. However,...
4.1K
Constant Volume Calorimetry02:41

Constant Volume Calorimetry

Calorimeters are useful to determine the heat released or absorbed by a chemical reaction. Coffee cup calorimeters are designed to operate at constant (atmospheric) pressure and are convenient to measure heat flow (or enthalpy change) accompanying processes that occur in solution at constant pressure. A different type of calorimeter that operates at constant volume, colloquially known as a bomb calorimeter, is used to measure the energy produced by reactions that yield large amounts of heat and...
30.6K
Leaky Scanning02:28

Leaky Scanning

During most eukaryotic translation processes, the small 40S ribosome subunit scans an mRNA from its 5' end until it encounters the first start AUG codon. The large 60S ribosomal subunit then joins the smaller one to initiate protein synthesis. The location of the translation initiation is largely determined by the nucleotides near the start codon as there may be multiple translation initiation sites present on the mRNA.  Marilyn Kozak discovered that the sequence RCCAUGG (where R...
5.7K