Related Experiment Video

Updated: Jan 23, 2026

Measuring the Strength of Mice
06:17

Measuring the Strength of Mice

Published on: June 2, 2013

56.5K

Chain-Shortened Myostatin Inhibitory Peptides Improve Grip Strength in Mice

Kentaro Takayama1, Tomo Asari1, Mariko Saitoh1

  • 1Department of Medicinal Chemistry and Department of Drug Delivery and Molecular Biopharmaceutics, Tokyo University of Pharmacy and Life Sciences, Hachioji, Tokyo 192-0392, Japan.

Related Concept Videos

Peptide Bonds02:43

Peptide Bonds

A peptide bond covalently attaches amino acids through a dehydration reaction. One amino acid's carboxyl group and another amino acid's amino group combine, releasing a water molecule. The resulting bond is the peptide bond. The products that such linkages form are peptides. As more amino acids join this growing chain, the resulting chain is a polypeptide. Each polypeptide has a free amino group at one end. This end has the N-terminal, or the amino-terminal, and the other end has a free...
82.5K
Acid Strength and Molecular Structure03:05

Acid Strength and Molecular Structure

Binary Acids and Bases
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
32.9K
Electron Transport Chains01:28

Electron Transport Chains

The final stage of cellular respiration is oxidative phosphorylation that consists of two steps: the electron transport chain and chemiosmosis. The electron transport chain is a set of proteins found in the inner mitochondrial membrane in eukaryotic cells. Its primary function is to establish a proton gradient that can be used during chemiosmosis to produce ATP and generate electron carriers, such as NAD+ and FAD, that are used in glycolysis and the citric acid cycle.
The ETC is comprised of...
111.8K
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
476
Relation Between Tensile Strength and Compressive Strength of Concrete01:30

Relation Between Tensile Strength and Compressive Strength of Concrete

Concrete is a fundamental building material, and understanding its strengths is crucial for construction projects. The relationship between its tensile and compressive strengths is intricate, showing that while these strengths are related, they do not increase at the same rate. Tensile strength's growth is slower and is affected by various factors such as the methods used for testing, the size and shape of the specimen, the texture of the aggregate used, and the moisture content of the...
658
The Equilibrium Binding Constant and Binding Strength02:18

The Equilibrium Binding Constant and Binding Strength

The equilibrium binding constant (Kb) quantifies the strength of a protein-ligand interaction. Kb can be calculated as follows when the reaction is at equilibrium:
14.9K