PYY is a negative regulator of bone mass and strength

Victoria D Leitch1, Mary Jane Brassill1, Sofia Rahman2

  • 1Molecular Endocrinology Laboratory, Department of Medicine, Hammersmith Campus, Imperial College London, London W12 0NN, United Kingdom.

Bone
|July 16, 2019
PubMed
Abstract

Related Concept Videos

Negative Regulator Molecules01:23

Negative Regulator Molecules

Positive regulators allow a cell to advance through cell cycle checkpoints. Negative regulators have an equally important role as they terminate a cell’s progression through the cell cycle—or pause it—until the cell meets specific criteria.
38.3K
Acid Strength and Molecular Structure03:05

Acid Strength and Molecular Structure

Binary Acids and Bases
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
32.9K
Relative Strengths of Conjugate Acid-Base Pairs02:29

Relative Strengths of Conjugate Acid-Base Pairs

Brønsted-Lowry acid-base chemistry is the transfer of protons; thus, logic suggests a relation between the relative strengths of conjugate acid-base pairs. The strength of an acid or base is quantified in its ionization constant, Ka or Kb, which represents the extent of the acid or base ionization reaction. For the conjugate acid-base pair HA / A−, the ionization equilibrium equations and ionization constant expressions are
51.4K
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
473
Relation Between Tensile Strength and Compressive Strength of Concrete01:30

Relation Between Tensile Strength and Compressive Strength of Concrete

Concrete is a fundamental building material, and understanding its strengths is crucial for construction projects. The relationship between its tensile and compressive strengths is intricate, showing that while these strengths are related, they do not increase at the same rate. Tensile strength's growth is slower and is affected by various factors such as the methods used for testing, the size and shape of the specimen, the texture of the aggregate used, and the moisture content of the...
656
The Equilibrium Binding Constant and Binding Strength02:18

The Equilibrium Binding Constant and Binding Strength

The equilibrium binding constant (Kb) quantifies the strength of a protein-ligand interaction. Kb can be calculated as follows when the reaction is at equilibrium:
14.9K