Related Experiment Video
Updated: Jan 22, 2026

Stress Distribution During Cold Compression of Rocks and Mineral Aggregates Using Synchrotron-based X-Ray Diffraction
Published on: May 20, 2018
Effect of different water-to-powder ratios on the dimensional stability and compressive strength of mineral
Eduardo Antunes Bortoluzzi1, Tchéli Cassel de Araújo1, Ana Carolina Corrêa Néis1
1Department of Dentistry - Endodontics Division, Health Sciences Center, Federal University of Santa Catarina,Florianópolis, SCBrazil.
Purpose:
The aim of this study was to evaluate the effect of different water-to-powder ratios on the dimensional stability and compressive strength of Portland cement and Mineral Trioxide Aggregate (MTA).
Materials And Methods:
Five different volumes of distilled water (0.26; 0.28; 0.30; 0.33 and 0.35 mL) were used for every 1 g of the cements. Twelve samples (12 mm long x 6 mm in diameter) were prepared in Teflon molds. After measuring the initial length, the specimens were stored in distilled water for 24 hours or 30 days. At the end of these time intervals, the specimens were measured again, and the dimensional change was calculated. The same samples used in the previous test were submitted to compression in a universal test machine (1 mm/min-1).
Results:
Analysis of the dimensional stability results showed no statistical difference between the cements, proportions and time intervals tested, or between their interactions. After 24 hours, MTA was more resistant than Portland cement (p<0.05). At 30 day-period, both cements had similar, and significantly higher resistance than they did at 24 hours (p<0.05).
Conclusion:
The powder/water ratio had no influence on the dimensional stability of cements. Compressive strength of Portland cement was affected at the proportions of 0.30 and 0.35 mL/g.
Related Concept Videos
Aggregate Cement Ratio
Water Cement Ratio
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Water and Mineral Acquisition
Relation Between Tensile Strength and Compressive Strength of Concrete