Related Experiment Video
Updated: Jan 22, 2026

Author Spotlight: Unveiling the Potential of VSFG Microscopy in Studying Mesoscopically Heterogeneous Self-Assembled Structures
Published on: December 1, 2023
Initial Growth Study of Atomic-Layer Deposition of Al2O3 by Vibrational Sum-Frequency Generation
V Vandalon1, W M M Erwin Kessels1
1Department of Applied Physics , Eindhoven University of Technology , P.O. Box 513, 5600 MB Eindhoven , The Netherlands.
Abstract:
The initial growth during the atomic-layer deposition (ALD) of Al2O3 using trimethylaluminum (TMA) and water was studied on two starting surfaces: SiO2 and -H-terminated Si(111) [H/Si(111)]. In situ spectroscopy ellipsometry (SE) showed virtually immediate growth of Al2O3 on both surfaces, although for H/Si(111) a reduced growth-per-cycle was observed in the initial 20 cycles. The underlying surface chemistry during the initial cycles of ALD was monitored with in situ broadband sum-frequency generation (BB-SFG) spectroscopy. For the SiO2 surface, the -CH3 surface groups were followed revealing that only the first TMA half-cycle deviates from the steady-growth regime. The reaction cross section of the initial TMA half-cycle (σTMA = 2.0 ± 0.2 × 10-18 cm2) was a factor of 3 lower than the cross section of the TMA half-cycle during the steady-growth regime of ALD (σTMA = 6.5 ± 0.6 × 10-18 cm2). All H2O half-cycles, including the first, showed steady-growth behavior with a corresponding reaction cross section (σH = 4.0 ± 0.4 × 10-20 cm2). Therefore, only the first ALD cycle was affected by initial growth effects on the SiO2 starting surface, in line with the SE data. For the H/Si(111) surface, the Si-H groups were monitored with BB-SFG spectroscopy, revealing a reaction cross section of σTMA = 3.1 ± 0.3 × 10-18 cm2 for the first TMA half-cycle on H/Si(111); a factor two lower than that during the steady regime of Al2O3. These results demonstrate that the chemistry during the initial growth regime of Al2O3 ALD on SiO2 and H/Si(111) shows subtle but measurable differences compared to the steady-growth regime.
More Related Videos
09:43Interfacial Molecular-level Structures of Polymers and Biomacromolecules Revealed via Sum Frequency Generation Vibrational Spectroscopy
Published on: August 13, 2019
09:45Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
Published on: July 26, 2016
Related Concept Videos
Atomic Mass
Atomic Nuclei: Larmor Precession Frequency
Sums of Power
Hybridization of Atomic Orbitals I
Wilcoxon Rank-Sum Test
Initiation of Translation
First, the initiator tRNA must be selected from the pool of elongator tRNAs by eukaryotic initiation factor 2 (eIF2). The initiator tRNA (Met-tRNAi) has conserved sequence elements including modified bases at...