Enhancement in Photoelectrochemical Performance of Optimized Amorphous SnS2 Thin Film Fabricated through Atomic Layer

Weiguang Hu1, Truong Thi Hien2, Dojin Kim2

  • 1Graduate School of Energy Science and Technology, Chungnam National University, Daejeon 305-764, Korea.

Related Concept Videos

Factors Affecting Dissolution: Polymorphism, Amorphism and Pseudopolymorphism01:21

Factors Affecting Dissolution: Polymorphism, Amorphism and Pseudopolymorphism

Polymorphism refers to the existence of a drug substance in multiple crystalline forms, known as polymorphs. Recently, this term has been expanded to include solvates (forms containing a solvent), amorphous forms (non-crystalline forms), and desolvated solvates (forms from which the solvent has been removed).
Some polymorphic crystals possess lower aqueous solubility than their amorphous counterparts, leading to incomplete absorption. For instance, the oral suspension of Chloramphenicol, which...
679
Atomic Structure01:33

Atomic Structure

Overview
207.3K
Atomic Mass01:52

Atomic Mass

Atoms — and the protons, neutrons, and electrons that compose them — are extremely small. For example, a carbon atom weighs less than 2 × 10−23 g. When describing the properties of tiny objects such as atoms, we use appropriately small units of measure, such as the atomic mass unit (amu). The amu was originally defined based on hydrogen, the lightest element, then later in terms of oxygen. Since 1961, it has been defined with regard to the most abundant isotope of carbon, atoms of which...
69.7K
Atomic Orbitals02:44

Atomic Orbitals

An atomic orbital represents the three-dimensional regions in an atom where an electron has the highest probability to reside. The radial distribution function indicates the total probability of finding an electron within the thin shell at a distance r from the nucleus. The atomic orbitals have distinct shapes which are determined by l, the angular momentum quantum number. The orbitals are often drawn with a boundary surface, enclosing densest regions of the cloud.
43.3K
Hybridization of Atomic Orbitals I03:24

Hybridization of Atomic Orbitals I

The mathematical expression known as the wave function, ψ, contains information about each orbital and the wavelike properties of electrons in an isolated atom. When atoms are bound together in a molecule, the wave functions combine to produce new mathematical descriptions that have different shapes. This process of combining the wave functions for atomic orbitals is called hybridization and is mathematically accomplished by the linear combination of atomic orbitals. The new orbitals that...
66.0K
The Energies of Atomic Orbitals03:21

The Energies of Atomic Orbitals

In an atom, the negatively charged electrons are attracted to the positively charged nucleus. In a multielectron atom, electron-electron repulsions are also observed. The attractive and repulsive forces are dependent on the distance between the particles, as well as the sign and magnitude of the charges on the individual particles. When the charges on the particles are opposite, they attract each other. If both particles have the same charge, they repel each other.
29.9K