A Coupled Experiment-finite Element Modeling Methodology for Assessing High Strain Rate Mechanical Response of Soft Biomaterials
Published on: May 18, 2015
Finite element simulation for the effect of loading rate on visco-hyperelastic characterisation of soft materials by
1Centre of Ultra-precision Optoelectric Instrument Engineering, Harbin Institute of Technology, Harbin, People's Republic of China. wangleiharbin@hit.edu.cn.
Abstract:
Nanoindentation test performed by atomic force microscopy is highly recommended for the characterisation of soft materials at nanoscale. The assumption proposed in the characterisation is that the material is pure elastic with no viscosity. However, this assumption does not represent the real characteristics of soft materials such as bio tissue or cell. Therefore, a parametric finite element simulation of nanoindentation by spherical tip was carried out to investigate the response of cells with different constitutive laws (elastic, hyperelastic and visco-hyperelastic). The investigation of the loading rate effect on the characterisation of cell mechanical properties was performed for different size of spherical tip. The selected dimensions of spherical tips cover commercially available products. The viscosity effects are insensitive to the varied dimensions of spherical tip in this study. A limit loading rate was found above which viscous effect has to be considered to correctly determine the mechanical properties. The method in this work can be implemented to propose a criterion for the threshold of loading rate when viscosity effect can be neglected for soft material characterisation.
Related Concept Videos
Spherical Coordinates
Elements and Compounds
Elements
Elements are classified as atomic or molecular based on the nature of their basic units. They are unique forms of matter with specific chemical and physical properties that cannot break down into smaller substances by ordinary chemical reactions. There...
Periodic Classification of the Elements
Classification of Elements and Compounds
Compounds are pure substances composed of two or more elements in fixed, definite proportions. Compounds are classified as ionic or molecular (covalent) based on the bonds...
Key Elements for Plant Nutrition
Spherical and Cylindrical Capacitor
Conventionally, considering the symmetry, the electric field between the concentric shells of a spherical capacitor is directed radially outward. The magnitude of the field,...