Atomic Layer Deposition of ZnO on CuO Enables Selective and Efficient Electroreduction of Carbon Dioxide to Liquid

Dan Ren1, Jing Gao1, Linfeng Pan2

  • 1Laboratory of Photonics and Interfaces, Institute of Chemical Sciences and Engineering, École Polytechnique Fédérale de Lausanne (EPFL), 1015, Lausanne, Switzerland.

Related Concept Videos

Carbon-dioxide Fixation01:28

Carbon-dioxide Fixation

Carbon dioxide fixation in prokaryotes enables the assimilation of inorganic carbon into organic molecules, supporting biosynthetic pathways, sustaining ecosystems, and contributing to the global carbon cycle. It also has industrial applications in carbon capture and bioproduct synthesis. Autotrophic organisms rely on this process to utilize CO₂ as a carbon source in diverse environments.The Calvin CycleThe Calvin cycle is the most widespread carbon fixation mechanism, primarily used by...
656
Carbon Dioxide Transport in the Blood01:19

Carbon Dioxide Transport in the Blood

Carbon dioxide (CO2) transport in the blood is critical to human physiology. On average, our body cells produce around 200 mL of CO2 per minute, precisely the quantity expelled by the lungs. This process involves the transportation of CO2 from the tissue cells to the lungs in three primary forms.
Forms of CO2 Transport
1. Dissolved in plasma: A small percentage (7-10%) of CO2 is transported and dissolved directly in the plasma.
2. Carbaminohemoglobin: Just over 20% of CO2 is chemically bound to...
4.8K
The Carbon Cycle01:14

The Carbon Cycle

Carbon is the basis of all organic matter on Earth, and is recycled through the ecosystem in two primary processes: one in which carbon is exchanged among living organisms, and one in which carbon is cycled over long periods of time through fossilized organic remains, weathering of rocks, and volcanic activity. Human activities, including increased agricultural practices and the burning of fossil fuels, has greatly affected the balance of the natural carbon cycle.
43.3K
Batteries and Fuel Cells03:12

Batteries and Fuel Cells

A battery is a galvanic cell that is used as a source of electrical power for specific applications. Modern batteries exist in a multitude of forms to accommodate various applications, from tiny button batteries such as those that power wristwatches to the very large batteries used to supply backup energy to municipal power grids. Some batteries are designed for single-use applications and cannot be recharged (primary cells), while others are based on conveniently reversible cell reactions that...
30.8K
Phase Transitions: Sublimation and Deposition02:33

Phase Transitions: Sublimation and Deposition

Some solids can transition directly into the gaseous state, bypassing the liquid state, via a process known as sublimation. At room temperature and standard pressure, a piece of dry ice (solid CO2) sublimes, appearing to gradually disappear without ever forming any liquid. Snow and ice sublimate at temperatures below the melting point of water, a slow process that may be accelerated by winds and the reduced atmospheric pressures at high altitudes. When solid iodine is warmed, the solid sublimes...
19.7K
Carbon Skeletons01:12

Carbon Skeletons

Life on Earth is carbon-based, as all macromolecules that make up living organisms contain carbon atoms. All organic compounds have a carbon backbone. Each carbon atom is tetravalent and can bond with four other atoms, making it an extraordinarily flexible component of biological molecules. Because carbon’s valence electrons are stable, it rarely becomes an ion. As the carbon chain increases in length, structural modifications such as ring structures, double bonds, and branching side...
114.2K