Nonlinear Etch Rate of Au-Assisted Chemical Etching of Silicon

Keorock Choi1,2, Yunwon Song1,2, Bugeun Ki1,2

  • 1School of Integrated Technology, Yonsei University, 85 Songdokwahak-ro, Yeonsu-gu, Incheon 21983, Republic of Korea.

ACS Omega
|August 29, 2019
PubMed

Related Concept Videos

Focused Ion Beam Lithography to Etch Nano-architectures into Microelectrodes13:49

Focused Ion Beam Lithography to Etch Nano-architectures into Microelectrodes

We have shown that the etching of nano-architecture into intracortical microelectrode devices may reduce the inflammatory response and has the potential to improve electrophysiological recordings. The methods described herein outline an approach to etch nano-architectures into the surface of non-functional and functional single shank silicon intracortical...
7.1K
Aesthetically Enhanced Silica Aerogel Via Incorporation of Laser Etching and Dyes08:21

Aesthetically Enhanced Silica Aerogel Via Incorporation of Laser Etching and Dyes

This protocol describes a method for etching text, patterns, and images onto the surface of silica aerogel monoliths in native and dyed form and assembling the aerogels into mosaic...
3.3K
Electrochemical Etching and Characterization of Sharp Field Emission Points for Electron Impact Ionization06:58

Electrochemical Etching and Characterization of Sharp Field Emission Points for Electron Impact Ionization

A method for electrochemically etching field emission tips is presented. Etching parameters are characterized and the operation of the tips in field emission mode is...
10.0K
Custom Engineered Tissue Culture Molds from Laser-etched Masters08:56

Custom Engineered Tissue Culture Molds from Laser-etched Masters

Herein we present a rapid, facile, and low-cost method for fabricating custom polydimethylsiloxane molds that can be used for producing hydrogel-based engineered tissues with complex geometries. We additionally describe results from mechanical and histological assessments conducted on engineered cardiac tissues produced using this...
6.8K
Fundamental Technical Elements of Freeze-fracture/Freeze-etch in Biological Electron Microscopy11:17

Fundamental Technical Elements of Freeze-fracture/Freeze-etch in Biological Electron Microscopy

Basic techniques and refinements of freeze-fracture processing of biological specimens and nanomaterials for examination by transmission electron microscopy are described. This technique is a preferred method for revealing ultrastructural features and specializations of biological membranes and for obtaining ultrastructural level dimensional and spatial data in materials sciences and nanotechnology...
34.1K
One-Step Approach to Fabricating Polydimethylsiloxane Microfluidic Channels of Different Geometric Sections by Sequential Wet Etching Processes08:31

One-Step Approach to Fabricating Polydimethylsiloxane Microfluidic Channels of Different Geometric Sections by Sequential Wet Etching Processes

Several methods are available for the fabrication of channels of non-rectangular sections embedded in polydimethylsiloxane microfluidic devices. Most of them involve multistep manufacturing and extensive alignment. In this paper, a one-step approach is reported for fabricating microfluidic channels of different geometric cross sections by polydimethylsiloxane sequential wet...
10.3K