Elucidation of Titanium Dioxide Nucleation and Growth on a Polydopamine-Modified Nanoporous Polyvinylidene Fluoride

Audra DeStefano1, Jiashi Yin1, Theodore J Kraus1

  • 1Department of Chemical Engineering and Chemistry Department, University of Wyoming, 1000 E. University Avenue, Laramie, Wyoming 82071, United States.

ACS Omega
|August 29, 2019
PubMed

Related Concept Videos

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model11:10

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

Thin films (100-1000 Å) of vanadium dioxide (VO2) were created by atomic-layer deposition (ALD) on sapphire substrates. Following this, the optical properties were characterized through the metal-insulator transition of VO2. From the measured optical properties, a model was created to describe the tunable refractive index of...
12.4K
Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition09:45

Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition

This work details the procedures for the growth and characterization of crystalline SrTiO3 directly on germanium substrates by atomic layer deposition. The procedure illustrates the ability of an all-chemical growth method to integrate oxides monolithically onto semiconductors for metal-oxide semiconductor...
12.8K
Growth of Gold Dendritic Nanoforests on Titanium Nitride-coated Silicon Substrates05:02

Growth of Gold Dendritic Nanoforests on Titanium Nitride-coated Silicon Substrates

This study presents a feasible procedure for synthesizing gold dendritic nanoforests on titanium nitride/silicon substrates. The thickness of gold dendritic nanoforests increases linearly within 15 min of a synthesis...
6.8K
Digital Printing of Titanium Dioxide for Dye Sensitized Solar Cells08:19

Digital Printing of Titanium Dioxide for Dye Sensitized Solar Cells

This paper investigates the suitability of inkjet printing for the manufacturing of dye-sensitized solar cells. A binder-free TiO2 nanoparticle ink was formulated and printed onto a FTO glass substrate. The printed layer was fabricated into a cell with an active area of 0.25 cm2 and an efficiency of...
13.2K
Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition14:01

Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition

Tin sulfide (SnS) is a candidate material for Earth-abundant, non-toxic solar cells. Here, we demonstrate the fabrication procedure of the SnS solar cells employing atomic layer deposition, which yields 4.36% certified power conversion efficiency, and thermal evaporation which yields...
43.3K
Assessing Disaster Resilience of Concrete with Titanium Dioxide Nanoparticles05:45

Assessing Disaster Resilience of Concrete with Titanium Dioxide Nanoparticles

This protocol describes the assessment of whether applying titanium dioxide to concrete enhances its physical properties, thereby increasing its resistance to the effects of natural disasters caused by extreme...
242