Related Experiment Video
Updated: Jan 20, 2026

How to Ignite an Atmospheric Pressure Microwave Plasma Torch without Any Additional Igniters
Published on: April 16, 2015
Great Variety of Man-Made Porous Diamond Structures: Pulsed Microwave Cold Plasma System with a Linear Antenna
Marián Varga1, Štepán Potocký1, Mária Domonkos1,2
1Institute of Physics, Czech Academy of Sciences, Cukrovarnická 10, 162 00 Prague 6, Czech Republic.
Abstract:
Synthetic diamond films are routinely grown using chemical vapor deposition (CVD) techniques. Due to their extraordinary combination of intrinsic properties, they are used as the functional layers in various bio-optoelectronic devices. It is a challenge to grow the dimensional layers or porous structures that are required. This study reviews the fabrication of various porous diamond-based structures using linear antenna microwave plasma (LAMWP) chemical vapor deposition (CVD), a low-cost technology for growing diamond films over a large area (>1 m2) at low pressure (<100 Pa) and at low temperature (even at 350 °C). From a technological point of view, two different approaches, i.e., templated diamond growth using three different prestructured (macro-, micro-, and nanosized) porous substrates and direct bottom-up growth of ultra-nanoporous diamond (block-stone and dendritelike) films, are successfully employed to form diamond-based structures with controlled porosity and an enhanced surface area. As a bottom-up strategy, the LAMWP CVD system allows diamond growth at as high as 80% CO2 in the CH4/CO2/H2 gas mixture. In summary, the low-pressure and cold plasma conditions in the LAMWP system facilitate the growth on three-dimensionally prestructured substrates of various materials that naturally form porous self-standing diamond structures.
Related Concept Videos
08:42How to Ignite an Atmospheric Pressure Microwave Plasma Torch without Any Additional Igniters
06:36Treating Surfaces with a Cold Atmospheric Pressure Plasma using the COST-Jet
07:17Non-equilibrium Microwave Plasma for Efficient High Temperature Chemistry
07:57Effect of Microwave Synthesis Conditions on the Structure of Nickel Hydroxide Nanosheets
06:12Plasma Polishing as a New Polishing Option to Reduce the Surface Roughness of Porous Titanium Alloy for 3D Printing
10:35Using Microwave and Macroscopic Samples of Dielectric Solids to Study the Photonic Properties of Disordered Photonic Bandgap Materials