Related Experiment Video
Updated: Jan 20, 2026

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
Published on: May 23, 2018
Atomic Layer Deposition of High-Quality Al2O3 Thin Films on MoS2 with Water Plasma Treatment
Binjie Huang1,2, Minrui Zheng1, Yunshan Zhao1
1Department of Electrical and Computer Engineering , National University of Singapore , 117583 , Singapore.
Abstract:
Atomic layer deposition (ALD) of ultrathin dielectric films on two-dimensional (2D) materials for electronic device applications remains one of the key challenges because of the lack of dangling bonds on the 2D material surface. In this work, a new technique to deposit uniform and high-quality Al2O3 films with thickness down to 1.5 nm on MoS2 is introduced. By treating the surface using water plasma prior to the ALD process, hydroxyl groups are introduced to the MoS2 surface, facilitating the chemisorption of trimethylaluminum in a conventional water-based ALD system. Raman and X-ray photoelectron spectroscopy measurements show that the water plasma treatment does not induce noticeable material degradation. The deposited Al2O3 films show excellent device-related electrical performance characteristics, including low interface trap density and outstanding gate controllability.
More Related Videos
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
09:45Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
Published on: July 26, 2016
Related Concept Videos
11:10Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited
Zn1-xMgxO
09:45Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
14:01Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition
08:49Atomically Defined Templates for Epitaxial Growth of Complex Oxide Thin Films
08:18Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application