Composition-Controlled Atomic Layer Deposition of Phase-Change Memories and Ovonic Threshold Switches with High

Valerio Adinolfi1, Lanxia Cheng1, Mario Laudato1

  • 1Intermolecular , 3011 North First Street , San Jose , California 95135 , United States.

ACS Nano
|September 5, 2019
PubMed

Related Concept Videos

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model11:10

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

Thin films (100-1000 Å) of vanadium dioxide (VO2) were created by atomic-layer deposition (ALD) on sapphire substrates. Following this, the optical properties were characterized through the metal-insulator transition of VO2. From the measured optical properties, a model was created to describe the tunable refractive index of...
12.4K
Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition14:01

Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition

Tin sulfide (SnS) is a candidate material for Earth-abundant, non-toxic solar cells. Here, we demonstrate the fabrication procedure of the SnS solar cells employing atomic layer deposition, which yields 4.36% certified power conversion efficiency, and thermal evaporation which yields...
43.3K
Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition09:45

Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition

This work details the procedures for the growth and characterization of crystalline SrTiO3 directly on germanium substrates by atomic layer deposition. The procedure illustrates the ability of an all-chemical growth method to integrate oxides monolithically onto semiconductors for metal-oxide semiconductor...
12.8K
Phase Transitions: Sublimation and Deposition02:33

Phase Transitions: Sublimation and Deposition

Some solids can transition directly into the gaseous state, bypassing the liquid state, via a process known as sublimation. At room temperature and standard pressure, a piece of dry ice (solid CO2) sublimes, appearing to gradually disappear without ever forming any liquid. Snow and ice sublimate at temperatures below the melting point of water, a slow process that may be accelerated by winds and the reduced atmospheric pressures at high altitudes. When solid iodine is warmed, the solid sublimes...
19.7K
Gradient Echo Quantum Memory in Warm Atomic Vapor10:00

Gradient Echo Quantum Memory in Warm Atomic Vapor

The gradient echo memory is a protocol for storing optical quantum states of light in atomic ensembles. Quantum memory is a key element of a quantum repeater, which can extend the range of quantum key distribution. We outline the operation of the scheme when implemented in a 3-level atomic...
13.2K
Layer-by-layer Collagen Deposition in Microfluidic Devices for Microtissue Stabilization09:56

Layer-by-layer Collagen Deposition in Microfluidic Devices for Microtissue Stabilization

The creation of functional microtissues within microfluidic devices requires the stabilization of cell phenotypes by adapting traditional cell culture techniques to the limited spatial dimensions in microdevices. Modification of collagen allows the layer-by-layer deposition of ultrathin collagen assemblies that can stabilize primary cells, such as hepatocytes, as microfluidic tissue...
9.8K