Related Experiment Video
Updated: Jan 6, 2026

Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
Strength Development and Strain Localization Behavior of Cemented Paste Backfills Using Portland Cement and Fly Ash
Yue Zhao1, Abbas Taheri2, Amin Soltani3
1School of Civil, Environmental and Mining Engineering, The University of Adelaide, Adelaide, SA 5005, Australia. Yue.Zhao@adelaide.edu.au.
Abstract:
This study examines the combined performance of Portland cement (PC), the binder, and fly ash (FA), the additive, towards improving the mechanical performance of the South Australian copper-gold underground mine cemented paste backfill (CPB) system. A series of unconfined compressive strength (UCS) tests were carried out on various mix designs to evaluate the effects of binder and/or additive contents, as well as curing time, on the CPB's strength, stiffness and toughness. Moreover, the failure patterns of the tested samples were investigated by means of the three-dimensional digital image correlation (DIC) technique. Making use of several virtual extensometers, the state of axial and lateral strain localization was also investigated in the pre- and post-peak regimes. The greater the PC content and/or the longer the curing period, the higher the developed strength, stiffness and toughness. The use of FA alongside PC led to further strength and stiffness improvements by way of inducing secondary pozzolanic reactions. Common strength criteria for CPBs were considered to assess the applicability of the tested mix designs; with regards to stope stability, 4% PC + 3% FA was found to satisfy the minimum 700 kPa threshold, and thus was deemed as the optimum choice. As opposed to external measurement devices, the DIC technique was found to provide strain measurements free from bedding errors. The developed field of axial and lateral strains indicated that strain localization initiates in the pre-peak regime at around 80% of the UCS. The greater the PC (or PC + FA) content, and more importantly the longer the curing period, the closer the axial stress level required to initiate localization to the UCS, thus emulating the failure mechanism of quasi-brittle materials such as rock and concrete. Finally, with an increase in curing time, the difference between strain values at the localized and non-localized zones became less significant in the pre-peak regime and more pronounced in the post-peak regime.
More Related Videos
05:38Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
06:27Expression of Cementitious Pore Solution and the Analysis of Its Chemical Composition and Resistivity Using X-ray Fluorescence
Published on: September 23, 2018
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Types of Cement II
Pozzolans
Fly ash is...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Soundness of Cement
Portland Cement