Microbial induced solidification and stabilization of municipal solid waste incineration fly ash with high alkalinity

Ping Chen1, Hao Zheng1, Hui Xu1

  • 1School of Civil Engineering and Architecture, Zhejiang Sci-Tech University, Hangzhou, China.

Plos One
|October 18, 2019
PubMed

Related Concept Videos

Pozzolans01:21

Pozzolans

Pozzolans are siliceous or aluminous materials blended with Portland cement. They interact with the calcium hydroxide produced during the hydration of Portland cement and contribute to improved strength and durability of concrete. The pozzolanic activity, a measure of a pozzolan's effectiveness, is typically assessed using the strength activity index, as defined in ASTM C 618-93, which calculates the ratio of the compressive strength of cement mixtures with and without pozzolan.
Fly ash is...
438
Coagulation01:06

Coagulation

Colloidal solids are solid particles suspended in solution. They are usually negatively charged, attracting a compact primary layer of positively charged ions, which attract more counterions to form an electrical double layer. Electrostatic repulsion between the charged double layers prevents the particles from colliding, stabilizing the colloids. These solids are often undesirable because they can contain toxins that are difficult to remove. Coagulation is a technique that helps aggregate and...
1.1K
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
438
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
642