Durable Antipilling Modification of Cotton Fabric with Chloropyrimidine Compounds
Xue Dong1, Tieling Xing2, Guoqiang Chen3
1National Engineering Laboratory for Modern Silk, College of Textile and Clothing Engineering, Soochow University, Suzhou 215123, China. dongxue@suda.edu.cn.
Abstract:
Cotton fabric, a natural cellulose material, is widely used in the textile industry for its excellent properties. However, its application in some fields are seriously restricted because of its poor antipilling behavior. In this study, cotton fabrics were modified with 2,4,6-trichloropyrimidine (TLP), 2,4-dichloro-5-methoxypyrimidine (DMP), and 2-amino-4,6-dichloropyridine (ADP). The surface morphology and chemical structure of the modified cotton fabric were characterized by scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD). Furthermore, the antipilling behavior, dyeing properties, thermal properties, and mechanical properties of modified cotton fabric were evaluated. The results showed that chloropyrimidine compounds were successfully grafted onto the surface of the cotton fabric, leading to excellent and durable antipilling activity of grade 3-4 even after 10 washes. Moreover, compared with control cotton fabric, the heat release rate (HRR) and total heat release (THR) of TLP-modified cotton fabric decreased to 173.2 W/g (42.3% reduction) and 11.3 KJ/g (13.7% reduction), respectively. In addition, the increased K/S value of modified cotton fabrics dyed with reactive dyes indicated that the modification can enhance the dyability of cotton fabric. This technique provides a simple and versatile method for improving the antipilling behavior of cellulosic materials and supports further preparation of functional textiles.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
Cationic Chain-Growth Polymerization: Mechanism