The Performance of Carbonation-Cured Concrete

Zhen Li1,2, Zhen He2, Xiaorun Chen2,3

  • 1School of Urban Construction, Yangtze University, No.1 Nanhuan Road, Jingzhou 434023, China.

Related Concept Videos

Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
408
Accelerated Curing of Concrete01:25

Accelerated Curing of Concrete

Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
409
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
321
Effects of Air-entrainment in Concrete01:28

Effects of Air-entrainment in Concrete

Air entrainment in concrete significantly enhances the material's durability, especially in environments subjected to freeze-thaw cycles. Introducing small air bubbles into the concrete mix acts as internal voids that accommodate the expansion of water when it freezes, thereby alleviating internal stress and preventing structural cracks. This function is crucial in climates with significant freezing and thawing, as it protects the concrete from repeated stresses that could lead to premature...
331
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
917
Curing Methods01:26

Curing Methods

Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...