Abstract:
In modern times, the Industry X.0 has emerged as the paradigm that has become the core of digital technology-driven business organizations. Further, this paper establishes a tube to tube plate friction welding technology with the help of deploying an external tool, also known referred to as the FWTPET scheme. Besides, the SA213 tube and SA387 tube plate were combined by employing a unique interference fit technique. Also, the strength of this combined portion was assessed with and without the aid of a holding block. Subsequently, the analytic optimization approaches like genetic algorithm, analysis of variance, and Taguchi L9 orthogonal array design were deployed in the prediction of the optimum joining strength. Moreover, the input parameters include the projection of the tube (mm), the rotational speed of the tool (rpm), and depth of cut (mm); besides, the tensile strength is considered as the output parameter. Also, the grain size distribution around the weld zone and the presence of base metal were measured through an optical microscope as per ASTM linear intercept method. Further, it is evident that grain refinement had occurred in the weld zone, which in turn increases the tensile strength. The exceptional weld strength (tensile strength) was obtained when joining of SA213 tube and SA387 tube plate through interference fit using a holding block without a hole in the tube. Experimentally, it was found that the achieved tensile strengths were 836.8 MPa (without a hole) and 789.35 MPa (with hole) using the holding block, respectively. Additionally, it was found that in the absence of a holding block, the achieved tensile strength is 762.2 MPa (without a hole), and 700.8 MPa (with a hole), correspondingly. The deviation of tensile strength between the predicted (genetic algorithm) and experimental was found minimal. Therefore, for achieving this strength, the suitable operating parameters set include the rotational speed of the tool (1300 rpm), projection of the tube (1 mm), and depth of cut (0.5 mm) with backing block configuration.
Related Concept Videos
Stresses under Combined Loadings
The process begins by slicing the tube at critical points and analyzing the internal forces and stress components at these sections, focusing on the centroid. Normal stresses, generated by axial forces and bending moments, are either compressive or tensile and vary across the section from...
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Temperature Dependent Deformation
Design of Transmission Shafts - Stress Analysis
Stress Concentrations in Circular Shafts
Relation Between Tensile Strength and Compressive Strength of Concrete