Thermodynamic insight into the thermoresponsive behavior of chitosan in aqueous solutions: A differential scanning

V Y Grinberg1, T V Burova2, N V Grinberg2

  • 1A.N. Nesmeyanov Institute of Organoelement Compounds, Russian Academy of Sciences, Vavilov St. 28, Moscow 119991, Russian Federation; N.M. Emanuel Institute of Biochemical Physics, Russian Academy of Sciences, Kosygin St. 4, Moscow 119991, Russian Federation.

Carbohydrate Polymers
|December 13, 2019