Related Experiment Video
Updated: Dec 30, 2025

Synthesis and Testing of Supported Pt-Cu Solid Solution Nanoparticle Catalysts for Propane Dehydrogenation
Published on: July 18, 2017
Synergetic effect on catalytic activity and charge transfer in Pt-Pd bimetallic model catalysts prepared by atomic
Moon-Hyung Jang1, Orhan Kizilkaya2, A Jeremy Kropf3
1Department of Chemical and Materials Engineering, University of Alabama in Huntsville, Huntsville, Alabama 35899, USA.
Abstract:
Pt-Pd bimetallic nanoparticles were synthesized on TiO2 support on the planar substrate as well as on high surface area SiO2 gel by atomic layer deposition to identify the catalytic performance improvement after the formation of Pt-Pd bimetallic nanoparticles by surface analysis techniques. From X-ray absorption near edge spectra of Pt-Pd bimetallic nanoparticles, d-orbital hybridization between Pt 5d and Pd 4d was observed, which is responsible for charge transfer from Pt to Pd. Moreover, it was found from the in situ grazing incidence X-ray absorption spectroscopy study that Pt-Pd nanoparticles have a Pd shell/Pt core structure with CO adsorption. Resonant photoemission spectroscopy on Pt-Pd bimetallic nanoparticles showed that Pd resonant intensity is enhanced compared to that of Pd monometallic nanoparticles because of d-orbital hybridization and electronic states broadening of Pt and Pd compared monometallic catalysts, which results in catalytic performance improvement.
Related Concept Videos
Catalysis
Reduction of Alkenes: Asymmetric Catalytic Hydrogenation
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...