The high-pressure, high-temperature phase diagram of cerium
K A Munro1, D Daisenberger2, S G MacLeod1,3,4
1SUPA, School of Physics and Astronomy and Centre for Science at Extreme Conditions, The University of Edinburgh, Peter Guthrie Tait Road, Edinburgh, EH9 3FD, United Kingdom.
Abstract:
We present an experimental study of the high-pressure, high-temperature behaviour of cerium up to ∼22 GPa and 820 K using angle-dispersive x-ray diffraction and external resistive heating. Studies above 820 K were prevented by chemical reactions between the samples and the diamond anvils of the pressure cells. We unambiguously measure the stability region of the orthorhombicoC4 phase and find it reaches its apex at 7.1 GPa and 650 K. We locate the α-cF4-oC4-tI2 triple point at 6.1 GPa and 640 K, 1 GPa below the location of the apex of theoC4 phase, and 1-2 GPa lower than previously reported. We find the α-cF4 →tI2 phase boundary to have a positive gradient of 280 K (GPa)-1, less steep than the 670 K (GPa)-1reported previously, and find theoC4 →tI2 phase boundary to lie at higher temperatures than previously found. We also find variations as large as 2-3 GPa in the transition pressures at which theoC4 →tI2 transition takes place at a given temperature, the reasons for which remain unclear. Finally, we find no evidence that the α-cF4 →tI2 is not second order at all temperatures up to 820 K.
Related Concept Videos
Phase Diagram
Phase Diagrams
Electron Configuration of Multielectron Atoms
pV-Diagrams
Heating and Cooling Curves
For instance, the addition of heat raises the temperature of a solid; the amount of heat absorbed depends on the heat capacity of the solid (q = mcsolidΔT). According to thermochemistry, the relation between the amount of heat absorbed or released by a substance, q, and its...
Phase Transitions