Related Experiment Video
Updated: Dec 26, 2025

Synthesis of Zeolites Using the ADOR Assembly-Disassembly-Organization-Reassembly Route
Published on: April 3, 2016
A Stable Silanol Triad in the Zeolite Catalyst SSZ-70
Christian Schroeder1,2, Christian Mück-Lichtenfeld3, Le Xu4
1Institut für Physikalische Chemie, Westfälische Wilhelms-Universität, Corrensstrasse 28/30, 48149, Münster, Germany.
Abstract:
Nests of three silanol groups are located on the internal pore surface of calcined zeolite SSZ-70. 2D 1 H double/triple-quantum single-quantum correlation NMR experiments enable a rigorous identification of these silanol triad nests. They reveal a close proximity to the structure directing agent (SDA), that is, N,N'-diisobutyl imidazolium cations, in the as-synthesized material, in which the defects are negatively charged (silanol dyad plus one charged SiO- siloxy group) for charge balance. It is inferred that ring strain prevents the condensation of silanol groups upon calcination and removal of the SDA to avoid energetically unfavorable three-rings. In contrast, tetrad nests, created by boron extraction from B-SSZ-70 at various other locations, are not stable and silanol condensation occurs. Infrared spectroscopic investigations of adsorbed pyridine indicate an enhanced acidity of the silanol triads, suggesting important implications in catalysis.
More Related Videos
09:37Imine Metathesis by Silica-Supported Catalysts Using the Methodology of Surface Organometallic Chemistry
Published on: October 18, 2019
09:46Adsorption Device Based on a Langatate Crystal Microbalance for High Temperature High Pressure Gas Adsorption in Zeolite H-ZSM-5
Published on: August 25, 2016
Related Concept Videos
Ziegler–Natta Chain-Growth Polymerization: Overview
Preparation and Reactions of Sulfides