Grain Growth Behavior of 0.95(Na0.5Bi0.5)TiO3-0.05BaTiO3 Controlled by Grain Shape and Second Phase
Sang-Chae Jeon1, John G Fisher2, Suk-Joong L Kang3
1School of Materials Science and Engineering, Changwon National University, 20 Changwondaehak-ro, Uichang-gu, Changwon, Gyeongsangnam 51140, Korea.
Abstract:
The grain growth behavior of 0.95(Na0.5Bi0.5)TiO3-0.05BaTiO3 (mole fraction, NBT-5BTdid not appear in any of the NBT-5BT samples with excess Bi2O3. The amount of liquid phase increased as the amount of Bi2O3 increased. Therefore, the rate of grain growth could be decreased by the increasing the distance for the diffusion of atoms. These observations allowed us to conclude that the growth of Bi2O3-excess NBT-5BT grains is governed by the growth of facet planes via the two-dimensional nucleation grain growth mechanism during changing grain shape and amount of liquid.
More Related Videos
Related Concept Videos
Crystal Growth: Principles of Crystallization
Initiating crystallization involves manipulating the concentration of the solute and the temperature of the solution. Since crystal growth occurs when the ratio of concentration and solubility of the solute in the solvent...
Precipitate Formation and Particle Size Control
The obtained precipitate should be either a pure substance of known composition or easily converted to one by a simple process, such as ignition or drying. In addition, the precipitate should be insoluble and easily filterable. In general, filterability...