Titanium alloy wire is characterized by high specific strength, good corrosion resistance, high-temperature resistance and other excellent comprehensive performance. It has been widely used not only in aerospace, shipbuilding and other high-tech fields, but also increasingly in medical equipment, food safety and other fields. Because titanium alloy wire is relatively difficult to process, it has a large deformation resistance, good elasticity, high flexion ratio and more serious rebound. During the processing, adhesion problems may occur, thus reducing the surface quality. The magnetic abrasive finishing (MAF) has good flexible machining characteristics. In this study, the rotating magnetic field was loaded on the titanium alloy wire, and the magnetic abrasive was absorbed by the magnetic field force to form a magnetic abrasive brush, so as to realize the precision processing of the titanium alloy wire. Under the same processing time, when the angle of the magnetic head was 37°, the surface roughness of titanium alloy wire was reduced to 0.28 μm by MAF, which improved the processing quality and efficiency of the titanium alloy wire.
Related Concept Videos
Magnetic Field Due To A Thin Straight Wire
Ferromagnetism
Magnetic Field Due to Two Straight Wires