Published on: August 8, 2025
High-Q Nanophotonic Resonators on Diamond Membranes using Templated Atomic Layer Deposition of TiO2
Amy Butcher1, Xinghan Guo1, Robert Shreiner2
1Pritzker School of Molecular Engineering, University of Chicago, Chicago, Illinois 60637, United States.
Abstract:
Integrating solid-state quantum emitters with nanophotonic resonators is essential for efficient spin-photon interfacing and optical networking applications. While diamond color centers have proven to be excellent candidates for emerging quantum technologies, their integration with optical resonators remains challenging. Conventional approaches based on etching resonators into diamond often negatively impact color center performance and offer low device yield. Here, we developed an integrated photonics platform based on templated atomic layer deposition of TiO2 on diamond membranes. Our fabrication method yields high-performance nanophotonic devices while avoiding etching wavelength-scale features into diamond. Moreover, this technique generates highly reproducible optical resonances and can be iterated on individual diamond samples, a unique processing advantage. Our approach is suitable for a broad range of both wavelengths and substrates and can enable high-cooperativity interfacing between cavity photons and coherent defects in diamond or silicon carbide, rare earth ions, or other material systems.
More Related Videos
10:28Fabrication of Nanopillar-Based Split Ring Resonators for Displacement Current Mediated Resonances in Terahertz Metamaterials
Published on: March 23, 2017
12:47Preparation and Use of Photocatalytically Active Segmented Ag|ZnO and Coaxial TiO2-Ag Nanowires Made by Templated Electrodeposition
Published on: May 2, 2014