Dataset for TiN Thin Films Prepared by Plasma-Enhanced Atomic Layer Deposition Using Tetrakis(dimethylamino)titanium

Woo-Jae Lee1, Eun-Young Yun1, Han-Bo-Ram Lee2

  • 1School of Materials Science and Engineering, Pusan National University, 30 Jangjeon-Dong Geumjeong-Gu, Busan, 609-735, Republic of Korea.

Data in Brief
|June 20, 2020