Copper leaching from waste printed circuit boards using typical acidic ionic liquids recovery of e-wastes' surplus
Ding-Jun Zhang1, Li Dong1, Yong-Tong Li1
1State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China.
Abstract:
In this study, using several types of acidic ionic liquids as the leaching reagents, the leaching behaviors of the copper present in waste printed circuit boards (WPCBs) were investigated. The effects of various parameters on the copper leaching rate were studied, such as the particle size of the shredded WPCB, type of ionic liquid used, hydrogen peroxide dosage, solid-to-liquid ratio, leaching temperature, and leaching time. The experimental results showed that the copper leaching rate increases continuously when the powder particle size is increased from 0.071 to 0.500 mm. Moreover, the copper leaching rate also increases with an increase in the leaching temperature. In contrast, the leaching rate first increases and then decreases with increases in the leaching time, hydrogen peroxide dosage, and solid-to-liquid ratio. The optimal conditions that provided a 98.31% copper leaching rate were: particle size >0.500 mm, 8.5 mL 90% (v/v) ionic liquid, 1.5 mL 30% hydrogen peroxide, solid-to-liquid ratio of 1/20, leaching temperature of 80 °C, and leaching time of 2 h.
More Related Videos
Related Concept Videos
Extraction: Advanced Methods
Electrodeposition
Electrodeposition can...
Precipitation and Co-precipitation
Voltaic/Galvanic Cells
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...