Effect of etching with low concentration hydrofluoric acid on the bond strength of CAD/CAM resin block

Yuiko Niizuma1, Mikihiro Kobayashi1, Toshinari Toyama1

  • 1Department of Conservative Dentistry, Division of Aesthetic Dentistry and Clinical Cariology, Showa University School of Dentistry.

Related Concept Videos

Acid Strength and Molecular Structure03:05

Acid Strength and Molecular Structure

Binary Acids and Bases
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
32.5K
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
419
Weak Acid Solutions04:02

Weak Acid Solutions

Few compounds act as strong acids. A far greater number of compounds behave as weak acids and only partially react with water, leaving a large majority of dissolved molecules in their original form and generating a relatively small amount of hydronium ions. Weak acids are commonly encountered in nature, being the substances partly responsible for the tangy taste of citrus fruits, the stinging sensation of insect bites, and the unpleasant smells associated with body odor. A familiar example of a...
41.6K
Calculating pH Changes in a Buffer Solution02:45

Calculating pH Changes in a Buffer Solution

A buffer can prevent a sudden drop or increase in the pH of a solution after the addition of a strong acid or base up to its buffering capacity; however, such addition of a strong acid or base does result in the slight pH change of the solution. The small pH change can be calculated by determining the resulting change in the concentration of buffer components, i.e., a weak acid and its conjugate base or vice versa. The concentrations obtained using these stoichiometric calculations can be used...
57.2K
Bonding and Strength of Aggregate01:12

Bonding and Strength of Aggregate

The bond between aggregate particles and the cement matrix is significantly influenced by the shape and surface texture of the aggregates. High-strength concretes benefit from a rougher texture, which leads to stronger bonding due to greater adhesion. Angular aggregates with larger surface areas also enhance this bond. The bonding quality, however, is complex to assess as no universally accepted test exists. Good bonding is indicated when a crushed concrete specimen shows some aggregate...
358
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
578