Biocement stabilization of an experimental-scale artificial slope and the reformation of iron-rich crusts

Alan Levett1, Emma J Gagen2, Yitian Zhao3

  • 1School of Earth and Environmental Sciences, University of Queensland, Brisbane, QLD 4072, Australia; alan.levett@uqconnect.edu.au.

Related Concept Videos

Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...
387
Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
376
Soundness of Cement01:17

Soundness of Cement

The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
410
Slump Test01:20

Slump Test

The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
674