Realization of an Ultrahigh Power Factor and Enhanced Thermoelectric Performance in TiS2 via Microstructural Texture
Yan Gu1, Kaikai Song1, Xiaohui Hu1
1College of Materials Science and Engineering, Nanjing Tech University, Nanjing 210009, China.
Abstract:
Layered 1T-type TiS2 powders were pretreated by an ethanol-based shear pulverization process, which showed outstanding effectiveness in reducing the average grain size and narrowing the size distribution while maintaining high crystallinity and plate-shaped morphology. The resulting bulk ceramics densified by spark plasma sintering possessed a highly (00l)-oriented texture and pronounced anisotropy. They showed a noticeably increased σ and an unaffected S in the in-plane direction due to the increased carrier mobility μ and the constant carrier concentration n, which resulted in a significant enhancement of the in-plane power factor, optimally to an unprecedented high level of 1.6-1.8 mW m-1 K-2 in a range of 323-673 K. Meanwhile, the lattice thermal conductivity was reduced by approximately 20% due to the intensified grain boundary phonon scattering that overwhelmed the effect due to texturing. These effects not only demonstrated the powder shear pulverization pretreatment as a facial and reliable route toward a high-textured TiS2 but also enabled a remarkable increase of ZT record for TiS2-based thermoelectrics (TEs) to approximately 0.7 at 673 K, indicating clearly the significant effect of texture engineering on TE performance.