Phosphate group adsorption capacity of inorganic elements affects bond strength between CAD/CAM composite block and
Eri Tokunaga1, Noriyuki Nagaoka2, Yukinori Maruo3
1Department of Occlusal and Oral Functional Rehabilitation, Graduate School of Medicine, Dentistry and Pharmaceutical Sciences, Okayama University.
Abstract:
This study aimed to investigate whether inorganic elements of polymer-infiltrated ceramic (PIC) and microfilled resin (MFR) for CAD/CAM would affect initial bond strength to luting agent. Inorganic elements of PIC and MFR were different with shape and ingredient observed by SEM, STEM and EDS. Microtensile bond strengths (µTBS) value of PIC was increased by 10-methacryloyloxydecyl dihydrogen phosphate (MDP) and acetic acid (AA)- or MDP-activated silane treatment, and further increased by succeeding heat treatment (HT). The µTBS of MFR was increased by MDP and MDP-activated silane, but decreased by AA-activated silane without HT. The HT improved the µTBS of MFR with AA-activated silane, but conversely for MDP-activated silane. Only in MFR, phosphoric acid (PA) application before each surface treatment dramatically decreased the µTBS of AA-activated silane. FTIR peaks in MFR shifted according to phosphate group's peak. MFR would possess high phosphate group adsorption capacity, with MDP effectively improving its bonding capability.
More Related Videos
Related Concept Videos
Complexometric Titration: Ligands
Bonding and Strength of Aggregate
EDTA: Chemistry and Properties
Essential Minerals for Bone Health
Calcium and Phosphorus
Calcium is a critical component of bones, especially in the form of calcium phosphate and calcium carbonate. Since the body cannot make calcium, it must be obtained from the diet. However, calcium cannot be absorbed from the small intestine without...
Factors Affecting Solubility
Complexation Equilibria: The Chelate Effect