Morphology Dependent Flow Stress in Nickel-Based Superalloys in the Multi-Scale Crystal Plasticity Framework
Shahriyar Keshavarz1, Zara Molaeinia2, Andrew C E Reid3
1National Institute of Standards and Technology/Theiss Research, 7411 Eads Ave, La Jolla, CA 92037, USA.
Abstract:
This paper develops a framework to obtain the flow stress of nickel-based superalloys as a function of γ-γ' morphology. The yield strength is a major factor in the design of these alloys. This work provides additional effects of γ' morphology in the design scope that has been adopted for the model developed by authors. In general, the two-phase γ-γ' morphology in nickel-based superalloys can be divided into three variables including γ' shape, γ' volume fraction and γ' size in the sub-grain microstructure. In order tfo obtain the flow stress, non-Schmid crystal plasticity constitutive models at two length scales are employed and bridged through a homogenized multi-scale framework. The multi-scale framework includes two sub-grain and homogenized grain scales. For the sub-grain scale, a size-dependent, dislocation-density-based finite element model (FEM) of the representative volume element (RVE) with explicit depiction of the γ-γ' morphology is developed as a building block for the homogenization. For the next scale, an activation-energy-based crystal plasticity model is developed for the homogenized single crystal of Ni-based superalloys. The constitutive models address the thermo-mechanical behavior of nickel-based superalloys for a large temperature range and include orientation dependencies and tension-compression asymmetry. This homogenized model is used to obtain the morphology dependence on the flow stress in nickel-based superalloys and can significantly expedite crystal plasticity FE simulations in polycrystalline microstructures, as well as higher scale FE models in order to cast and design superalloys.
More Related Videos
Related Concept Videos
Stress-Strain Diagram - Ductile Materials
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Plastic Behavior
Plastic Deformations
Stress-Strain Diagram - Brittle Materials
Plastic Deformations of Members with a Single Plane of Symmetry