Creep Testing of Thermoplastic Fiber-Reinforced Polymer Composite Tubular Coupons
Hai Giang Minh Doan1, Pierre Mertiny1
1Department of Mechanical Engineering, University of Alberta, 9211-116 St., Edmonton, AB T6G 1H9, Canada.
Abstract:
Thermoplastic fiber-reinforced polymer composites (TP-FRPC) are gaining popularity in industry owing to characteristics such as fast part fabrication, ductile material properties and high resistance to environmental degradation. However, TP-FRPC are prone to time-dependent deformation effects like creep under sustained loading, which can lead to significant dimensional changes and affect the safe operation of structures. Previous research in this context has focused, mainly, on testing of flat coupons. In this study, a creep testing method for TP-FRPC tubular coupons was developed. Specimens were fabricated using tape winding and subjected to well-defined loading conditions, i.e., pure hoop tensile and pure axial compressive stress. Strain gauges and digital image correlation were both employed for strain measurements and were found to be in good agreement. The evolution of strain rate, Poisson's ratio and creep compliance were investigated. The prediction of experimental data by the Burgers model and the Findley's power law model were explored. The research findings suggest that the developed experimental and analysis approach provides valuable information for the design of material systems and structures.
More Related Videos
08:40Ultrasonic Welding of Thermoplastic Composite Coupons for Mechanical Characterization of Welded Joints through Single Lap Shear Testing
Published on: February 11, 2016
09:54Author Spotlight: Enhancing Fiber Composite Laminate Quality with the Wet Hand Lay-Up/Vacuum Bag Process
Published on: June 30, 2023
Related Concept Videos
Fiber Reinforced Concrete
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Creep in Concrete
Factors Affecting Creep
Further, the water/cement ratio is critical, as a lower ratio increases concrete strength, thus reducing creep. The strength of the...