Isomerization and Selective Hydrogenation of Propyne: Screening of Metal-Organic Frameworks Modified by Atomic Layer
Ryan A Hackler, Riddhish Pandharkar1, Magali S Ferrandon
1Department of Chemistry, Chemical Theory Center, and Supercomputing Institute, University of Minnesota-Twin Cities, 207 Pleasant Street SE, Minneapolis, Minnesota 55455, United States.
Abstract:
Various metal oxide clusters upward of 8 atoms (Cu, Cd, Co, Fe, Ga, Mn, Mo, Ni, Sn, W, Zn, In, and Al) were incorporated into the pores of the metal-organic framework (MOF) NU-1000 via atomic layer deposition (ALD) and tested via high-throughput screening for catalytic isomerization and selective hydrogenation of propyne. Cu and Co were found to be the most active for propyne hydrogenation to propylene, and synergistic bimetallic combinations of Co and Zn, along with standalone Zn and Cd, were established as the most active for conversion to the isomerized product, propadiene. The combination of Co and Zn in NU-1000 diminished the propensity for full hydrogenation to propane as well as coking compared to its individual components. This study highlights the potential for high-throughput screening to survey monometallic and bimetallic cluster combinations that best affect the efficient transformation of small molecules, while discerning mechanistic differences in isomerization and hydrogenation by different metals.
Related Concept Videos
Reduction of Alkenes: Asymmetric Catalytic Hydrogenation
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...
Reduction of Alkynes to cis-Alkenes: Catalytic Hydrogenation
Like alkenes, alkynes can be reduced to alkanes in the presence of transition metal catalysts such as Pt, Pd, or Ni. The reaction involves two sequential syn additions of hydrogen via a cis-alkene intermediate.
Reduction of Alkenes: Catalytic Hydrogenation
Metals like palladium, platinum, and nickel are commonly used in their solid forms — fine powder on an inert surface. As these catalysts remain insoluble in the reaction mixture, they are referred to as heterogeneous catalysts.
The hydrogenation process takes place on the...
Preparation of Alkynes: Dehydrohalogenation
Alkynes can be prepared by dehydrohalogenation of vicinal or geminal dihalides in the presence of a strong base like sodium amide in liquid ammonia. The reaction proceeds with the loss of two equivalents of hydrogen halide (HX) via two successive E2 elimination reactions.
Alkynes to Aldehydes and Ketones: Hydroboration-Oxidation
One of the convenient methods for the preparation of aldehydes and ketones is via hydration of alkynes. Hydroboration-oxidation of alkynes is an indirect hydration reaction in which an alkyne is treated with borane followed by oxidation with alkaline peroxide to form an enol that rapidly converts into an aldehyde or a ketone. Terminal alkynes form aldehydes, whereas internal alkynes give ketones as the final product.
Alkynes to Aldehydes and Ketones: Acid-Catalyzed Hydration
Analogous to alkenes, alkynes also undergo acid-catalyzed hydration. While the addition of water to an alkene gives an alcohol, hydration of alkynes produces different products such as aldehydes and ketones.